Polymer Property : Electrical Resistivity = 300000 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 300000 ohm-cm
300000 ohm-cm
Shakespeare Resistat® F901 N022 Nylon 6 Monofilament
Resistat F901, MERGE N022 is a 22-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of ..
Electrical Resistivity 300000 ohm-cm
300000 ohm-cm
Shakespeare Resistat® F901 S022 Nylon 6 Monofilament
Resistat F901, MERGE S022 is a 33-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of ..
Electrical Resistivity 300000 ohm-cm
300000 ohm-cm
Shakespeare Resistat® F9122 A400 Nylon 6 Monofilament
Resistat F9122, MERGE A400 is a 22 denier per filament, 4 inch, conductive nylon 6 stable. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cr..
Electrical Resistivity 300000 ohm-cm

@Temperature 1000 °C
300000 ohm-cm

@Temperature 1830 °F
ASTM D1829
CoorsTek Mullite, S2
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..