Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.20e+10 - 3.90e+12 ohm-cm | 2.20e+10 - 3.90e+12 ohm-cm | Average value: 7.76e+11 ohm-cm Grade Count:19 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |