Polymer Property : Electrical Resistivity = 3.80e+17 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 - 3.80e+17 ohm-cm
10.0 - 3.80e+17 ohm-cm
Average value: 2.29e+16 ohm-cm Grade Count:43
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..