Electrical Properties Metric English Comments
Electrical Resistivity 3.20e+15 ohm-cm
3.20e+15 ohm-cm
Momentive Performance Materials RTV656 Clear Extreme Low Temperature Potting/Encapsulating Compound
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
Electrical Resistivity 3.20e+15 ohm-cm
3.20e+15 ohm-cm
ASTM D257
Ascend Performance Materials VYDYNE® 45 Nylon, Impact Modified, Weather Stable
Typical property data. VYDYNE is a registered trademark of Solutia Inc.