Polymer Property : Electrical Resistivity = 3.10e+12 ohm-cm
Polymer Property :
Electrical Resistivity =
3.10e+12 ohm-cm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Electrical Resistivity
3.10e+12
ohm-cm
3.10e+12
ohm-cm
GBC Grade 97 Alumina
Data provided by the manufacturer, GBC Materials Corporation.