Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.90 - 3.00e+17 ohm-cm | 1.90 - 3.00e+17 ohm-cm | Average value: 1.46e+16 ohm-cm Grade Count:94 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Electrical Resistivity | 5.00 - 3.00e+17 ohm-cm | 5.00 - 3.00e+17 ohm-cm | Average value: 4.97e+15 ohm-cm Grade Count:117 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |