Polymer Property : Electrical Resistivity = 3.00e+17 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 3.00e+17 ohm-cm
3.00e+17 ohm-cm
ASTM D257
LyondellBasell Alathon® M6080WC High Density Polyethylene
ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c..