Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 8.30e+11 - 3.00e+13 ohm-cm | 8.30e+11 - 3.00e+13 ohm-cm | Average value: 1.04e+13 ohm-cm Grade Count:9 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |