Electrical Properties Metric English Comments
Electrical Resistivity 2.80e+14 ohm-cm
2.80e+14 ohm-cm
Momentive Performance Materials RTV88 Red Extreme High Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..