Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 2.50e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 2.50e+16 ohm-cm
2.50e+16 ohm-cm
ASTM D257
Plenco 51240 PET, Pellet, Injection Molded, Green  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..