Polymer Property : Electrical Resistivity = 2.50e+10 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 2.50e+10 ohm-cm

@Temperature 350 °C
2.50e+10 ohm-cm

@Temperature 662 °F
Momentive Performance Materials Type 219 Fused Quartz Tubing
Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran..