Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.42e+15 ohm-cm | 2.42e+15 ohm-cm | |
Abatron AboCast 50-11/AboCure 50-1 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 240 min. at 25°C(77°F). Exothermic Peak 190°C (375°F). Hardens in 2-24 hours.. |