Polymer Property : Electrical Resistivity = 2.30e+17 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 2.30e+17 ohm-cm
2.30e+17 ohm-cm
DuPont™ Kapton® 150FN019 Polyimide/FEP Composite Film
150 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r..