Electrical Resistivity 1.00e+14 - 2.20e+16 ohm-cm
1.00e+14 - 2.20e+16 ohm-cm
Average value: 8.01e+15 ohm-cm Grade Count:8
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..