Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | |
Cookson Group Plaskon® SMT-B-1RC (146.403) Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
Electrical Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | Compound; IE 600093 |
Borealis Casico™ FR4805 Non Halogen Flame Retardant Compound for Sheathing Energy Cables Casico FR4805 is a thermoplastic, non-halogen containing natural jacketing compound. It combines high mechanical strength and toughness with flame retardancy. The composition of Casico FR4805 is b.. |