Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
Plenco 5440 Black General Purpose Phenolic Molding Compound
(discontinued **) Plaslok 5440 is the replacement material for the former Union Carbide BMRS-5440. It is a two-stage, phenolic molding compound that has been successfully formulated to accommodate a very wide range .. |
|||
Electrical Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | |
GBC Grade 96 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Electrical Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
Toyobo Pelprene™ S-1001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Electrical Resistivity | 2.00e+12 ohm-cm | 2.00e+12 ohm-cm | ASTM D257 |
Plaslok 5440 Black General Purpose Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5440 is the replacement material for .. |