Electrical Resistivity 1e+11 ohm-cm
1e+11 ohm-cm
at 100V
PPT FP140 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Electrical Resistivity 1e+11 ohm-cm
1e+11 ohm-cm
at 100V
PPT FP150 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Electrical Resistivity 1e+11 ohm-cm
1e+11 ohm-cm
at 100V
PPT FP160 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..