Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 16700 ohm-cm | 16700 ohm-cm | |
BASF Theroplast® F Yellow 084 Color Additive Chemical Structure: PeryleneApplication: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BASF |