Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 120000 ohm-cm | 120000 ohm-cm | |
Shakespeare Resistat® F901 R055 Nylon 6 Monofilament Resistat F901, MERGE R055 is a 55-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of .. |