Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | >= 1100 ohm-cm | >= 1100 ohm-cm | |
BASF Sicotan® Red L 2817 Color Additive Description: Transparent red iron oxideChemical Structure: Iron-III-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Amine curing system and Airdr.. |