Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+14 - 1.30e+18 ohm-cm | 1.00e+14 - 1.30e+18 ohm-cm | Average value: 8.45e+16 ohm-cm Grade Count:17 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |