Electrical Properties Metric English Comments
Electrical Resistivity 1.10e+15 ohm-cm
1.10e+15 ohm-cm
ASTM D257
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Electrical Resistivity 1.10e+15 ohm-cm
1.10e+15 ohm-cm
Momentive Performance Materials RTV11 White General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Electrical Resistivity 1.10e+15 ohm-cm
1.10e+15 ohm-cm
Momentive Performance Materials RTV567 Translucent Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..