Polymer Property : Electrical Resistivity = 0.400 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.400 ohm-cm
0.400 ohm-cm
Poco Graphite SUPERSiC® Basic Silicon Carbide
The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for..
Electrical Resistivity 0.400 ohm-cm
0.400 ohm-cm
Poco Graphite SUPERSiC® Si Silicon Carbide
The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for..