Electrical Properties Metric English Comments
Electrical Resistivity 0.069 ohm-cm
0.069 ohm-cm
Standard
Touchstone CFOAM® 20 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..