Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0110 - 0.0330 ohm-cm | 0.0110 - 0.0330 ohm-cm | |
Heraeus Cleviosâ„¢ P Jet HC Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet HC is an antistatic material based on PE.. |
|||
Electrical Resistivity | 0.0110 - 0.0330 ohm-cm | 0.0110 - 0.0330 ohm-cm | |
Heraeus Cleviosâ„¢ P Jet N Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PT2 is an antistatic material based on PEDOT:P.. |