Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 0.00400 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00400 ohm-cm
0.00400 ohm-cm
Poco Graphite SUPERSiC® 3C Silicon Carbide
SUPERSiC that has been coated with a 75 µm CVD SiC coating, which seals the surface.Uses: Ideal for high-temperature deposition and CVD applications.Information provided by PocoGraphite
Electrical Resistivity 0.00400 ohm-cm
0.00400 ohm-cm
Poco Graphite SUPERSiC® 3CX Silicon Carbide
SUPERSiC that has been coated twice with a 75 µm CVD SiC coating, which seals the surface. Uses: Ideal for high-temperature anneal processesInformation provided by PocoGraphite
Electrical Resistivity 0.00400 ohm-cm
0.00400 ohm-cm
Poco Graphite SUPERSiC® Si-3C Silicon Carbide
SUPERSiC that has been infiltrated with silicon and then coated with a 75 µm CVD SiC coating, sealing off the porosity.Uses: Ideal for high-temperature vacuum CVD systemsInformation provided by Poc..
Electrical Resistivity 0.00400 - 0.00700 ohm-cm
0.00400 - 0.00700 ohm-cm
Alliance BIN-40 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00400 - 0.00700 ohm-cm
0.00400 - 0.00700 ohm-cm
Alliance BIN-26 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00400 - 0.00700 ohm-cm
0.00400 - 0.00700 ohm-cm
Alliance BIN-45 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00400 - 0.00700 ohm-cm
0.00400 - 0.00700 ohm-cm
Alliance BIN-48 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00400 - 0.00700 ohm-cm
0.00400 - 0.00700 ohm-cm
Alliance BIN-55 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00400 - 0.00700 ohm-cm
0.00400 - 0.00700 ohm-cm
Alliance BIN-72 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00400 ohm-cm
0.00400 ohm-cm
Poco Graphite SUPERSiC® Si-8C Silicon Carbide
SUPERSiC that has been infiltrated with silicon and then coated with a 200 µm CVD SiC coatingUses: Ideal for optical and lithography componentsInformation provided by Poco Graphite