Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00280 ohm-cm | 0.00280 ohm-cm | |
Poco Graphite SCF Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Electrical Resistivity | 0.00280 ohm-cm @Temperature 17.0 °C |
0.00280 ohm-cm @Temperature 62.6 °F |
in plane |
Carlisle 201LD Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |