Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00156 ohm-cm | 0.00156 ohm-cm | |
Poco Graphite EDM-3 EDM Graphite POCO's EDM-3 is an isotropic Ultrafine grain graphite which offers high strength with outstanding wear and fine surface finish characteristics easily machined to thicknesses of .005 or less.Applicat.. |
|||
Electrical Resistivity | 0.00156 ohm-cm | 0.00156 ohm-cm | |
Poco Graphite TRA Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |