Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00146 ohm-cm | 0.00146 ohm-cm | |
Poco Graphite Glassmate® SR Graphite An economical material for short production runs. An ideal insert material for thick bead transfer applications. |