Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00135 ohm-cm | 0.00135 ohm-cm | |
Ohio Carbon Blank OCB AR-12 EDM Grade Graphite Available in a range of sizes and shapes. |
|||
Electrical Resistivity | 0.00135 ohm-cm | 0.00135 ohm-cm | |
Ohio Carbon Blank OCB UT-3 Mechanical Grade Graphite Available in a range of sizes and shapes. |
|||
Electrical Resistivity | 0.00135 ohm-cm @Temperature 17.0 °C |
0.00135 ohm-cm @Temperature 62.6 °F |
in plane |
Carlisle 201HD Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |