Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000784 ohm-cm | 0.000784 ohm-cm | |
Lucas-Milhaupt Silvaloy® A35 Brazing Alloy Silvaloy A35 is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is used for brazing in the electrical industry and for brazing brass.. |