Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000500 ohm-cm | 0.000500 ohm-cm | |
Von Roll Isola IMI E-Solder® 3017 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Electrical Resistivity | 0.000500 ohm-cm | 0.000500 ohm-cm | |
Von Roll Isola IMI E-Solder® 3012 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Electrical Resistivity | 0.000500 ohm-cm | 0.000500 ohm-cm | |
Epoxyset Epoxiohm EO-21M-5 Electrically Conductive Epoxy Adhesive EO-21M-5 is an electrically conductive & thermally conductive, silver filled epoxy adhesive. This two component system is designed to be cured at room temperature or the cure can be accelerated by e.. |