Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000355 - 0.000365 ohm-cm | 0.000355 - 0.000365 ohm-cm | Unsintered |
FiberNide Nickel Aluminide Foam Atomic 15% Aluminum Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f.. |