Electrical Properties Metric English Comments
Electrical Resistivity 0.000140 ohm-cm

@Temperature 500 °C
0.000140 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000140 ohm-cm

@Temperature 500 °C
0.000140 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000140 ohm-cm

@Temperature 500 °C
0.000140 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000140 ohm-cm

@Temperature 500 °C
0.000140 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000140 ohm-cm

@Temperature 500 °C
0.000140 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000140 ohm-cm

@Temperature 500 °C
0.000140 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000140 ohm-cm

@Temperature 500 °C
0.000140 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000140 ohm-cm

@Temperature 500 °C
0.000140 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® B-3® alloy, 6.3 mm plate
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000140 ohm-cm

@Temperature 500 °C
0.000140 ohm-cm

@Temperature 932 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..