Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000117 ohm-cm | 0.000117 ohm-cm | |
Special Metals INCOLOY® Alloy 925 A precipitation-hardenable nickel-iron-chromium alloy with additions of molybdenum and copper. It combines the high strength of a precipitation-hardenable alloy with the excellent corrosion resista.. |