Electrical Properties Metric English Comments
Electrical Resistivity 0.000102 ohm-cm
0.000102 ohm-cm
Outokumpu 4762 High Temperature Ferritic Stainless Steel
Highest chromium content-most resistant to reducing sulphurous gases. Susceptible to 475°C embrittlement and s-phase forms during long exposures in the range 600-800°C.Applications: Mostly used i..
Electrical Resistivity 0.000102 ohm-cm
0.000102 ohm-cm
Temperature coefficient of resistance is 330 µOhm/Ohm-°C in the range 25-500°C.
Special Metals BRIGHTRAY® Alloy 35 Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 1920°F (1050°C). It is similar to BRIGHTRAY alloy F but with rare-earth additions for greater resist..
Electrical Resistivity 0.000102 ohm-cm
0.000102 ohm-cm
Special Metals NI-SPAN-C® Alloy 902
A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo..
Electrical Resistivity 0.000102 ohm-cm
0.000102 ohm-cm
Special Metals UDIMET® alloy 188 Cobalt-base Alloy
UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small ..
Electrical Resistivity 0.000102 ohm-cm

@Temperature 300 °C
0.000102 ohm-cm

@Temperature 572 °F
Special Metals INCOLOY® Alloy 903
A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a..