Polymer Property : Electrical Resistivity = 0.0000820 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000820 ohm-cm
0.0000820 ohm-cm
Crucible Steel XM-19 Stainless Steel
Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio..
Electrical Resistivity 0.0000820 ohm-cm
0.0000820 ohm-cm
Carlson Nitronic® 50® Austenitic Stainless Steel
General DescriptionNitronic 50 is a nitrogen-strengthened austenitic stainless steel that possesses corrosion resistance superior to 316, 316L, 317 and 317L plus approximately twice the yield streng..
Electrical Resistivity 0.0000820 ohm-cm
0.0000820 ohm-cm
Temperature Coefficient = 0.0011
Carpenter Invar 36® Alloy, Annealed Bars and Strip
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
Electrical Resistivity 0.0000820 ohm-cm
0.0000820 ohm-cm
Temperature Coefficient = 0.0011
Carpenter Invar 36® Alloy, Cold Drawn Bars
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
Electrical Resistivity 0.0000820 ohm-cm
0.0000820 ohm-cm
Temperature Coefficient = 0.0011
Carpenter Invar 36® Alloy, Cold Rolled Strip
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
Electrical Resistivity 0.0000820 ohm-cm
0.0000820 ohm-cm
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition TH 1050
AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va..