Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000707 ohm-cm | 0.0000707 ohm-cm | 3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02 |
Hoskins Manufacturing Chromel® Thermocouple Wire Used in Type E and Type K thermocouples. All values may vary dependent on specific design and usageChromel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsu.. |