Polymer Property : Electrical Resistivity = 0.0000695 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000695 ohm-cm
0.0000695 ohm-cm
AK Steel 301 Austenitic Stainless steel
AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach..