Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000685 ohm-cm | 0.0000685 ohm-cm | |
AK Steel 201 Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Electrical Resistivity | 0.0000685 ohm-cm | 0.0000685 ohm-cm | |
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |