Electrical Properties Metric English Comments
Electrical Resistivity 0.0000670 ohm-cm

@Temperature 23.0 °C
0.0000670 ohm-cm

@Temperature 73.4 °F
Crucible Steel 446 Chromium Steel
Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201, 10% Cold Work (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201, 40% Cold Work (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201, 5% Cold Work (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201, 50% Cold Work (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103)
Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese ..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201L, 20% Cold Work (UNS S20103)
Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese ..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201L, 5% Cold Work (UNS S20103)
Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese ..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201L, 50% Cold Work (UNS S20103)
Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese ..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201L, 60% Cold Work (UNS S20103)
Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese ..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201L, Annealed (UNS S20103)
Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese ..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201, 20% Cold Work (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201, 30% Cold Work (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201L, 30% Cold Work (UNS S20103)
Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese ..
Electrical Resistivity 0.0000670 ohm-cm
0.0000670 ohm-cm
ATI Allegheny Ludlum Stainless Steel Type 201L, 40% Cold Work (UNS S20103)
Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese ..