Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 0.0000600 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000500 - 0.0000600 ohm-cm
0.0000500 - 0.0000600 ohm-cm
Alliance S-20A Samarium Cobalt Magnetic Material
Electrical Resistivity 0.0000500 - 0.0000600 ohm-cm
0.0000500 - 0.0000600 ohm-cm
Alliance S-20B Samarium Cobalt Magnetic Material
Electrical Resistivity 0.0000500 - 0.0000600 ohm-cm
0.0000500 - 0.0000600 ohm-cm
Alliance S-26A Samarium Cobalt Magnetic Material
Electrical Resistivity 0.0000500 - 0.0000600 ohm-cm
0.0000500 - 0.0000600 ohm-cm
Alliance S-22A Samarium Cobalt Magnetic Material
Electrical Resistivity 0.0000500 - 0.0000600 ohm-cm
0.0000500 - 0.0000600 ohm-cm
Alliance S-22B Samarium Cobalt Magnetic Material
Copyright © lookpolymers.com All Rights Reserved