Electrical Properties Metric English Comments
Electrical Resistivity 0.0000587 ohm-cm
0.0000587 ohm-cm
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel
Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab..
Electrical Resistivity 0.0000587 ohm-cm
0.0000587 ohm-cm
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy
Allegheny Ludlum stainless Type AL 441HP™ alloy is a heat resisting ferritic grade providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dua..