Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000450 ohm-cm | 0.0000450 ohm-cm | |
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1) Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties.. |
|||
Electrical Resistivity | 0.0000450 ohm-cm | 0.0000450 ohm-cm | Temperature Coefficient of 0.0034/K |
Goodfellow Nickel 52/Iron 48 Alloy Used in magnetic and glass-metal seal applicationInformation provided by Goodfellow. |