Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Annealed and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | Aged |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | Aged |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | Aged |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | Aged |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | |
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 o.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | Aged |
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | Aged |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | Aged |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the .. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | Aged |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gener.. |
|||
Electrical Resistivity | 0.0000424 ohm-cm | 0.0000424 ohm-cm | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in gen.. |