Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000300 ohm-cm | 0.0000300 ohm-cm | |
Momentive Performance Materials Niobium Carbide (NbC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Electrical Resistivity | 0.0000300 ohm-cm | 0.0000300 ohm-cm | |
Momentive Performance Materials Tantalum Carbide (TaC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Electrical Resistivity | 0.0000300 ohm-cm | 0.0000300 ohm-cm | |
ATI Allegheny Ludlum Relay Steels No. 2 Silicon and iron alloyApplications:relays, armatures, solenoids, magnetic clutches, pole pieces, certain types of motors, transformers, data processing equipment.Information provided by Allegheny Lu.. |