Polymer Property : Electrical Resistivity = 0.00002234 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00002234 ohm-cm
0.00002234 ohm-cm
Williams Advanced Alloys WS280B Solder (Au80/Sn20)
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Electrical Resistivity 0.00002234 ohm-cm
0.00002234 ohm-cm
Williams Advanced Alloys WS292 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Electrical Resistivity 0.00002234 ohm-cm
0.00002234 ohm-cm
Williams Advanced Alloys WS305 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys