Polymer Property : Electrical Resistivity = 0.0000192 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000184 - 0.0000192 ohm-cm
0.0000184 - 0.0000192 ohm-cm
Temperature Coefficient of 0.0017/K
Goodfellow Platinum 90/Rhodium 10 Thermocouple Alloy
The positive element of the type S thermocouple. Type S thermocouples are characterized by a high degree of chemical inertness and stability at high temperatures. Often used as a standard for calibr..