Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000162 ohm-cm | 0.0000162 ohm-cm | Annealed |
Eagle Brass 725 Copper Nickel Tin, 1/2 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Electrical Resistivity | 0.0000162 ohm-cm | 0.0000162 ohm-cm | Annealed |
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Electrical Resistivity | 0.0000162 ohm-cm | 0.0000162 ohm-cm | Annealed |
Eagle Brass 725 Copper Nickel Tin, Annealed Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Electrical Resistivity | 0.0000162 ohm-cm | 0.0000162 ohm-cm | Annealed |
Eagle Brass 725 Copper Nickel Tin, Extra Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Electrical Resistivity | 0.0000162 ohm-cm | 0.0000162 ohm-cm | Annealed |
Eagle Brass 725 Copper Nickel Tin, Extra Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Electrical Resistivity | 0.0000162 ohm-cm | 0.0000162 ohm-cm | Annealed |
Eagle Brass 725 Copper Nickel Tin, Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Electrical Resistivity | 0.0000162 ohm-cm | 0.0000162 ohm-cm | Annealed |
Eagle Brass 725 Copper Nickel Tin, Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |