Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00001445 ohm-cm | 0.00001445 ohm-cm | |
Williams Advanced Alloys WS179 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Electrical Resistivity | 0.00001445 ohm-cm | 0.00001445 ohm-cm | |
Williams Advanced Alloys WS226 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Electrical Resistivity | 0.00001445 ohm-cm | 0.00001445 ohm-cm | |
Williams Advanced Alloys WS240 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |